Features include:
• 2” nominal seam height
• Typically 18” and narrower panel widths
• Continuous length panels
• Flat, ribbed or striations between the seams
• Common metals:
- Standard 24 gauge and 22 gauge steel,
- 16 and 20 ounce copper,
- 0.7mm and 0.8mm and 1.0mm zinc,
- 26 and 24 gauge stainless,
- 22 gauge rusting steel (cold-rolled, COR-TEN)
- Titanium
• Minimum slope 2:12 with endlaps
• UL Class 90 wind uplift rating for 24 gauge minimum thickness steel
• ASTM E1592 tested
• Air & Water infiltration tested |
• ASTM E2140 Static waster tested